Solventless output depends on a step most operators do by habit: how the bag is packed. Bag choice, fill volume, micron and the pressure ramp all interact, and the right answer is different for each input material. Get it wrong and you get slippage, blowouts and choked flow. Get it right and the same press produces more, more consistently.
This is a working reference for four material types.
1. Dried material
Dried material is the most forgiving input. It grips inside the bag, so slippage and blowouts are rare.
- Micron: 110 µm to 160 µm
- Volume per bag: 12 g to 28 g
- Bag count: typically 1 per press
- Bag thickness: thinner bags suit the lower output, keeping the channel gap open for flow
- Typical output: 10% to 20%
Temperature of 190°F to 210°F, depending on the material type and its condition. Pressure should start light and ramp gradually — blowouts come from fast ramps at high temperature. Time matters least here, because the material grips and does not slip; balance pressure against temperature instead.
One bag per press keeps cost per gram down, since fewer consumables are consumed per cycle.
2. Dry-sieved material
Dry-sieved input is a higher concentration of fine material, which makes the press more efficient and more consistent.
- Micron: 32 µm to 90 µm
- Volume per bag: 10 g to 40 g
- Bag count: usually 1; 2 if you are seeing slippage
- Bag thickness: thin, to keep flow open at low output volumes
- Typical output: 20% to 40%
Temperature of 160°F to 190°F preserves the volatile fractions. Pressure moderate and sustained — let the material flow rather than forcing it. Time is not critical, but let the material fully liquefy before going to full pressure.
3. Washed material, dried
Dried washed material behaves much like the two above: stable, not greasy, not especially prone to slipping. The pressure window is what differs.
- Micron: 32 µm
- Volume per bag: 15 g
- Bag count: 1, or 2 for more sensitive batches
- Bag thickness: thin, to avoid restricting flow
- Typical output: 20%
Temperature of 160°F to 180°F. Pressure from 300–500 psi, ramping to 1,000–1,500 psi — this material is stable enough to take the higher peak, and ramping rather than jumping avoids forcing particulate through with the flow. Time is again secondary to a gradual ramp.
4. Washed material, fresh-frozen
The most demanding input. Its greasy texture makes it far more prone to slipping and blowouts, so it needs tighter control of all three variables — and two bags, every time.
- Micron: 32 µm to 73 µm
- Volume per bag: 30 g to 50 g
- Bag count: always 2 per press
- Bag thickness: thicker pouches suit the higher volumes, but do not overpack
- Typical output: 70% to 95%
Temperature of 140°F to 170°F, kept low to retain volatile fractions. Pressure moderate, and patient — let it flow before applying full pressure. Time genuinely matters here: rushing the ramp is what causes slippage.
Double-bagging costs more per cycle. The higher output offsets it.
What bag count does to cost per gram
Bag count is the consumable line in your cost model. One bag per press is the cheaper cycle; two is necessary for fresh-frozen washed material and unavoidable if you want to avoid blowouts. The calculation is not "which is cheaper" but which material you are running — and for fresh-frozen, the higher output is what pays for the second bag.
Pressure, time and temperature together
Pressure. Stable inputs — dried, dry-sieved, dried washed — tolerate faster ramps and higher peaks, up to 1,000–1,500 psi for dried washed material. Fresh-frozen washed material needs a light start and a slow climb.
The safety window. It matters most for fresh-frozen: lower temperature and a slower ramp are what prevent slippage. The other three tolerate a more aggressive approach.
Packing well is not a craft secret. It is four variables, and knowing which of them your material actually cares about.